47 Carrington Road
Marrickville NSW 2204
Application:
PHASE | % W/W | RAW MATERIAL | QTY |
gms per Kg | |||
A | 59.4 | DEIONISED WATER | 594 |
0.1 | DISODIUM EDTA | 1 | |
30 | AMMONIUM LAURYL SULFATE 30% | 300 | |
1. ADD TO AMMONIUM LAURYL SULFAE SLOWLY TO THE WATER WITH HIGH SPEED STIRRING (PROPELLOR TYPE) | |||
B | 1.5 | CETYL ALCOHOL | 15 |
2. ADD THE CETYL ALCOHOL AND HEAT TO 65 - 70c. | |||
3. BEGIN COOLING (AND MIXING) TO 35 - 40c. | |||
4. MIX UNTIL UNIFORM. ALLOW AIR TO DISSAPATE BEFORE PROCEEDING. | |||
C | 5 | COCOAMIDOPROPYL BETAIN | 50 |
1 | PLANTASERV P | 10 | |
5. ADD PHASE C TO THE BATCH. | |||
6. MIX UNTIL UNIFORM. | |||
D | 2.5 | COCOAMIDE DEA | 25 |
0.25 | QUATERNIUM 80 | 2.5 | |
0.25 | NEEM OIL | 2.5 | |
7. PREMIX PHASE D AND ADD TO THE BATCH. | |||
8. MIX UNTIL UNIFORM. | |||
E | LACTIC ACID | 0 | |
TRIETHANOLAMINE | 0 | ||
9. ADJUST pH TO 5.75 - 6.25 (Note; Mix for 10 mins after each addoition). | |||
10. COOL TO ROOM TEMPERATURE | |||
F | SODIUM CHLORIDE | 0 | |
11. ADJUST VISCOSITY TO DESIRED LEVL WITH SALT. | |||
G | DEIONISED WATER | 0 | |
12. ADJUST VOLUME/WEIGHT TO COMPENSATE FOR WATER LOSS DURING MANUFACTURE | |||
TOTAL | 100 | 1000 |