PHASE | % W/W | RAW MATERIAL | QTY |
gms per Kg | |||
A | 59.4 | DEIONISED WATER | 594 |
0.1 | DISODIUM EDTA | 1 | |
2 | GLYCERINE | 20 | |
1. HEAT PHASE A TO 70 - 75°C. | |||
B | 4.5 | SUNFLOWER OIL | 45 |
0.5 | MACADAMIA NUT OIL | 5 | |
4.5 | BEESWAX | 45 | |
0.5 | SHEA BUTTER | 5 | |
0.5 | CETOMACROGOL 1000 | 5 | |
5 | EMULSIFYING WAX | 50 | |
3 | GLYCERYL STEARATE | 30 | |
2. HEAT PHASE B TO 70 - 75°C | |||
3. ADD PHASE B TO PHASE A USING SILVERSON FOR 10MIN | |||
4. COOL TO 45 - 50°C | |||
5. CHANGE TO SWEEP ACTION | |||
6. COOL TO 35 - 40°C | |||
C | 1 | PLANTASERV Q | 10 |
5 | COLLOIDAL OATMEAL | 50 | |
5 | CALAMINE BP | 50 | |
5 | AUSTRALIAN CLAY - IVORY | 50 | |
4 | ALOE VERA JUICE | 40 | |
7. ADD PHASE C INGREDIENTS TO BATCH (ONE AT A TIME) | |||
D | LACTIC ACID | 0 | |
TRIETHANOLAMINE | 0 | ||
8. ADJUST pH TO 5.0 to 6.0 | |||
9. COOL TO ROOM TEMPERATURE | |||
E | DEIONISED WATER | 0 | |
10. ADJUST VOLUME/WEIGHT TO COMPENSATE FOR WATER LOSS DURING MANUFACTURE | |||
TOTAL | 100 | 1000 |